Effect of Water-Air Microemulsion of Flotation Agent Solution on Flotation of Polymetallic Sulfide Ores

2022

Full text Open access: Gold Metadata (CSL-JSON)
DOI 10.3390/min12121612
Data confidence 70 medium
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

The enrichment of polymetallic sulfide ore is a complex task. Fine grinding is carried out to reveal useful minerals, resulting in the formation of microparticles. It is difficult to achieve the floatation of microparticles and fine useful minerals are lost with flotation tailings. The problem of microparticle flotation can be solved by using air bubbles smaller than 50 µmin for the flotation process. Water-air microemulsion (WAME)of a frothersolution obtained using the generator was used as microbubbles. The effect of WAME on flotation was studied on polymetallic ores and gold-bearing ore from Kazakhstan deposits.The use of WAMEin the processing of polymetallic ore allowed for themaintenance of the quality of rougher concentrates, to increase the copper extraction in Cu-Pb rougherconcentrate by 7.41%, of lead by 5.98% in the copper-lead flotation cycle (Cu-Pb-Zn-Fe ore), copper extraction in Cu-Mo rougherconcentrate by 5.2%, and molybdenum by 4.7% in the copper-molybdenum flotation cycle (Cu-Mo ore). The indicators of flotation gold extraction into the gold-containing concentrate significantly improved in comparison with the basic mode when using the generator in rougher and scavenger flotation cycles: the quality increased by 5.3 g/t, and the extraction increased by 4.27%.