THE EFFECT OF THE FRACTIONAL COMPOSITION OF CARBON ENRICHMENT WASTE ON THE PROPERTIES OF CERAMIC WALL MATERIALS

2023

Closed access Metadata (CSL-JSON)
DOI 10.55956/czdp5801
Data confidence 70 medium
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

Қарағанды және Екібастұз көмір кен орындарының көмірді байыту қалдықтарының химиялық, минералогиялық және химиялық құрамы зерттелді. Көмірді байыту қалдықтарын 0,14-0,315 мм аз ұнтақтау кезінде қажетті қалыптау және күйдіру қасиеттеріне қол жеткізілгені анықталды. Үлгілерді 1000оС температурада күйдіру кезінде жоғары беріктік мәндеріне және суды сіңірудің жеткілікті төмен көрсеткіштеріне қол жеткізіледі. Пісімделу температурасының 1050оС дейін жоғарылауы сығылу беріктігін одан әрі арттыруға және судың сіңуін төмендетуге көмектеседі. 0,63 мм фракциясы үшін үлгілердің максималды беріктігі 17,1 МПа, 0,315 мм фракциясы үшін – 22,7 МПа, 0,14 мм фракциясы үшін 25,4 МПа ,су сіңірімділік сәйкесінше 15,6, 13,4 және 12,2% құрайды