Analysis of Different Types of Carbonaceous Reductants and Methods of Slag and Sludge Recovery at Converter Production

2023

Closed access Metadata (CSL-JSON)
DOI 10.52209/1609-1825_2023_1_73
Data confidence 70 medium
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

Recycling of metal-containing wastes with an iron content of more than 15%, such as slag and sludge from the gas cleaning of converter production, can be used to recover the metal. In order to study the reducing properties of coal sludge, coke breeze (coke), Shubarkol coal, a series of experimental melting of coal sludge briquettes with different contents of the listed carbon-containing materials was carried out. Sludge-coal briquettes were made from converter slag and sludge using hydrated lime as a binder. To determine the necessary parameters for the reduction of the iron-containing element, chemical and technical analyzes were carried out for ash content, moisture content and volatile matter. The choice of the optimal component composition of briquetted mixtures has established that the proportion of the reducing agent in the briquette should not exceed 20...25%, in order to avoid excess carbon, which binds into solid carbide compounds. The share of the reducing agent in the briquette was 15...18%. Chemical analysis of the resulting alloy and slag component pointed out the expediency of using Shubarkol coal as a carbonaceous reducing agent with high reactivity and electrical resistivity