It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

The synthesized SrSO4 crystalline powders were irradiated at photon energies from 6 ÷ 12 eV, in the temperature range from 15 ÷ 300 K. The investigation was carried out by the methods of atomic absorption, luminescence and vacuum ultraviolet spectroscopy. Intrinsic emissions were found at 3.7-3.8 eV, 4.2-4.6 eV and 4.9-5 eV, and long-wavelength recombination emissions at 2.6-2.7 eV and 2.9-3.0 eV.The synthesized SrSO4 crystalline powders were irradiated at photon energies from 6 ÷ 12 eV, in the temperature range from 15 ÷ 300 K. The investigation was carried out by the methods of atomic absorption, luminescence and vacuum ultraviolet spectroscopy. Intrinsic emissions were found at 3.7-3.8 eV, 4.2-4.6 eV and 4.9-5 eV, and long-wavelength recombination emissions at 2.6-2.7 eV and 2.9-3.0 eV.