Study of Adhesion–Cohesive Interactions of Modified Bitumen Compositions

2025

Full text Open access: Gold Metadata (CSL-JSON)
DOI 10.3390/polym17020199
Data confidence 70 medium
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

The aim of the work was to study the effect of additive concentration on changes in the adhesive and cohesive strength of bitumen. To evaluate the effectiveness of modifiers in the composition of binary and triple bitumen systems in relation to mineral fillers of two grades, the method of determination of the adhesive efficiency and thermodynamic calculations of adhesion and cohesion work were used. The following compounds were used as additives: AS-2 synthesized from the oil refining waste and AG-4I (waste sealing liquid). Adhesion–cohesion processes in modified bitumen systems are limited by the wetting effect of crushed stone and the intensity of intermolecular forces in the condensed phase of the binder. In the binary compositions, the addition of modifiers into bitumen significantly improves the cohesive strength and adhesive efficiency in relation to crushed stone. The introduction of AS-2 into bitumen compositions with AG-4I increases adhesion efficiency and thermodynamic work of adhesion in relation to the filler surface. The adhesion efficiency and thermodynamic work of adhesion in the “bitumen-AG-4I-AS-2” system reach their maximum at CAG-4I = 3.0 g/dm3 and CAS-2 = 1.5 g/dm3. In these concentration modes, the composition ensures maximum increase in adhesion efficiency (AKS = 65.18%; AKA = 48.11%) and the greatest increase in thermodynamic work of adhesion (WA(KS) = 15.79 mN/m; WA(KA) = 14.13 mN/m).