Recovery of “Hard-to-Recover” Selenate Ions in Sulfuric Acid Solutions during Polarization of Titanium Electrodes by Industrial Alternating Current

Inorganics, 2022

Full text Open access: Gold Metadata (CSL-JSON)
DOI 10.3390/inorganics10060072
Data confidence 70 medium
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

The article is devoted to the study of selenium (VI) reduction processes in sulfuric acid solutions when titanium electrodes are polarized by alternating current of industrial frequency (50 Hz). It was found that selenate ion reduction occurs on the surface of titanium electrodes in the cathode half-cycle of alternating current (practically at the cathode) by reaction: SeO42−+ 6e + 8H+ → Se + 4H2O. In addition, the recovery is carried out by titanium (III) ions: 6Ti3+ SeO42−+ 8H+ → Se + 6Ti4+ + 4H2O. It has been established that titanium (III) ions are products of dissolution of titanium during polarization by alternating current, so they can be formed by reaction: 2Ti + 6H+ → 2Ti3+ + 3H2. Reduction in selenate ions during polarization by alternating current can also occur due to the cementation reaction with titanium: 3Ti + 2SeO42− + 16H+ → 2Se + 8H2O + 3Ti4+. It was shown for the first time that the selenate ion is reduced to form a dispersed selenium powder with a high current efficiency. Depending on the conditions, both amorphous and crystalline selenium modifications are produced.