Thermoelectric properties of SiGe whiskers with various morphology

2017

Closed access Metadata (CSL-JSON)
DOI 10.1117/12.2280895
Data confidence 70 medium
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

Thermoelectric properties of Si1-xGex (x = 0.03) solid solution whiskers doped with B impurities to the concentrations 1017 – 1019 cm-3 were studied in temperature range 300 - 420K. An influence of the whisker morphology, in particular their diameters and obliquity, on Seebeck coefficient, thermal conductivity and resistance was investigated. Seebeck coefficient and resistance was shown to increase, while thermal conductivity to decrease when the whisker diameter drops from 100 to 10μm, that is accompanied by a rise of figure of merit (up to 0,12 at 300K). Use of the whiskers with large obliquity leads to a small rise (of about 10 – 15%) increase of their Seebeck coefficient.