Desorption of hydrogen from Ni—Cu—Cr catalyst on (θ + α-Al2O3 sorbent modified with cerium

2010

Closed access Metadata (CSL-JSON)
DOI 10.1134/s0036024410030234
Data confidence 70 medium
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

We present the results of thermal desorption studies of H 2 interactions with 8.9% Ni—Cu—Cr (1:3:0.1)/(θ+α)-Al 2 O 3 +2% Ce. It was demonstrated that three forms of hydrogen with different desorption temperatures and T max peak values are formed in the catalyst at 673 K: H 2 (ads), H(ads), and dissolved hydrogen. It was found that upon an increase in the adsorption temperature from 673 to 1173 K, H 2 (ads) and H(ads) remain on the surface (E des = 14.4 kcal/mol, first order desorption reaction, H: Ni = 1.6—1.88) while hydrogen dissolution in the Ni lattice and its copper alloy increases (E des = 32.9 kcal/mol, second order desorption reaction, H: Ni = 2.0).