It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

This paper describes the results of laboratory tests with samples of a new generation self-compacting fine-grained refractory concrete (self-flow castables -SFC refractory equivalent to self-compacting concrete -SCC) and tests of the properties of products made of the developed compositions.The tests were conducted with cube specimens 100x100x100 mm in size for developed SFC and prism specimens 40x40x160 mm in size for cement pastes.Laboratory tests were conducted to determine the residual strength after heating to 800°С and the ability of specimens to withstand sharp changes in temperature from 800°С to 20°С in water.A new method for selecting the composition by using main structural-rheological criteria (see section 3.1) was applied: ratio in volume of water-concrete dispersive mixture (rheological matrix of the first kind) over the absolute volume of fine sand /and ratio in volume of dispersive fine-grained mixture (rheological matrix of the second kind) over the absolute volume in sand-aggregateIt is shown that one of the ways to reduce the negative impact of high temperatures on the physical-mechanical properties of refractory concrete that uses Portland cement is the addition of the three slags components, that have equal thermal-expansion coefficient, amorphous silica fume of 10-15% of the cement mass.The project was conducted from February 2012 to February 2013.