It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

In this work, consider the aspects of obtaining powder coatings that possessing certain working properties obtained by detonation spraying. Experimental research were carried on the effect of technological parameters of the detonation spraying process on the phase composition and properties of Ti-Si-C coatings. It is determined that when the volume of filling the detonation barrel with an explosive mixture increases to 70% in the detonation wave flow, the Ti 3 SiC 2 powder partially decomposes into TiC consequently the high-speed shock interaction of heated to high temperatures. Installed that when filling the barrel with an explosive mixture of 50% and 60%, a low extent of decomposition of Ti 3 SiC 2 powder can be achieved. It is determined that an increase in the volume content of the TiC phase in the composition of coatings bring to a decrease in the hardness of the Ti-C-Si coating.