Bitumen Extraction from Bituminous Sands by Ultrasonic Irradiation

ChemEngineering, 2025

Full text Open access: Gold Metadata (CSL-JSON)
DOI 10.3390/chemengineering9050109
Data confidence 70 medium
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

This paper discusses the efficiency of ultrasonic-assisted bitumen extraction from bituminous sands of the Beke deposit (Mangistau region, Kazakhstan) using alkaline aqueous solutions. The process parameters, including ultrasonic frequency (22 kHz), power (up to 1500 W), solution pH (>12), and optimal NaOH concentration (1 wt.%) were optimized to achieve a maximum bitumen recovery of 98 wt.% within 8 min. The most effective sand-to-solution mass ratio was determined as 1:2, while the optimal process temperature was 75 °C. The application of ultrasound significantly enhances cavitation and reagent penetration, enabling efficient separation of bitumen with minimal chemical usage. Fourier-transform infrared (FTIR) spectroscopy and GC–MS analyses revealed the presence of aromatic hydrocarbons, paraffinic and naphthenic structures, as well as sulfur- and oxygen-containing functional groups (e.g., sulfoxides, carboxylic acids). These characteristics suggest moderate maturity and a high degree of aromaticity of the organic matter. Despite suitable thermal and compositional properties, the extracted bitumen exhibits a relatively low stiffness and softening point, indicating the need for additional upgrading (e.g., oxidation) prior to use in road construction. Although standard rheological tests (e.g., dynamic shear rhinometry) were not conducted in this study, the penetration and softening point values suggest a relatively soft binder, possibly unsuitable for high-temperature paving applications without modification. Future research will focus on rheological evaluation and oxidative upgrading to meet the ST RK 1373-2013 specification requirements.