It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

One of the most popular alloys for biomedical applications is TiAl6V4. Even though TiAl6V4 is widely used, it faces several challenges. Firstly, TiAl6V4 is prone to stress shielding caused by the difference in Young’s moduli of the alloy (110 GPa) and human bones (20–30 GPa). Secondly, there is the presence of cytotoxic elements, aluminum and vanadium. Researchers have proposed Ti-35Nb-7Zr-5Ta (TNZT) alloy to overcome these disadvantages, an excellent substitute for natural human bones. This alloy offers a lower elastic modulus (up to 81 GPa), much closer to human bones than TiAl6V4 alloy. Also, TNZT alloy contains no cytotoxic elements and has excellent biocompatibility and high corrosion resistance. Given the positive outcomes on powder-mixed micro electro-discharge machining (PM-μ-EDM) of Ti alloy using hydroxyapatite (HA) powder, we studied the machinability of TNZT alloy using HA powder mixed-μ-EDM by changing the HA powder concentration (0, 5, and 10 g/L), gap voltage (90, 100, and 110 V), and capacitance (10, 100, and 400 nF) according to the Taguchi L9 method. Machining performance metrics such as material removal rate (MRR), overcut, and circularity were examined using a tungsten carbide tool of 237 µm diameter. The results showed an overcut of 10.33 µm, circularity of 8.47 µm, and MRR of 6030.89 µm3/s for the lowest energy setup.