Coke Quality in Medium-Temperature Coking of Fractionated Long-Flame Coal

2022

Closed access Metadata (CSL-JSON)
DOI 10.3103/s1068364x22080051
Data confidence 70 medium
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

To improve the medium-temperature coking of fractionated long-flame Shubarkol coal (Kazakhstan) in vertical furnaces, the influence of the coking characteristics on coke quality is studied. Specifically, the influence of the following factors on the piece size, mechanical strength, and physicochemical properties of the coke is investigated: the coal’s piece size (25–100 and 25–80 mm), the final temperature (750 and 850°C), the heating rate (1.9–9.7°C/min), and the method of coke quenching. Industrial experience in the operation of various vertical furnaces with variation in heating conditions is briefly reviewed. Coking conditions for long-flame Shubarkol coal at the Shubarkol Komir plant are recommended for the production of high-quality carbon reducing agents that may be used in ferroalloy production. Possible applications of medium-temperature coke are considered.