Influence of Intermittent Quenching and Self-Tempering on the Mechanical Properties of Rebar Steel

2018

Closed access Metadata (CSL-JSON)
DOI 10.3103/s0967091218020079
Data confidence 70 medium
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

The influence of deformation and heat treatment on the mechanical properties of rebar steel is investigated on a pilot system. Specifically, with intermittent quenching and subsequent self-tempering, the intense-cooling time determines the tempering temperature of the quenched steel and hence the final mechanical properties of the rebar. The influence of the water pressure in the intense-cooling chamber on the uniformity of the mechanical properties is studied for steel with 0.31, 0.32, and 0.35% C; the water pressure is varied from 0.2 to 0.6 MPa. On that basis, it is established that the water pressure in the cooling chamber must be no less than 0.3 MPa, and the carbon content in the steel must be more than 0.32% in order to ensure that the mechanical properties of the rebar steel conform to the AT500 strength class according to State Standard GOST 10884–2004.