Complex Processing tailings of the Balkhash Concentrating Factory

2015

Full text Open access: Hybrid Metadata (CSL-JSON)
DOI 10.13005/bbra/1918
Data confidence 70 medium
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

At flotation concentration of copper ores the tailings are formed, which contain both nonferrous metals and a significant amount of silicon and iron.The nonferrous metals from the tailings can be taken by flotation or leaching; but the silicon and iron is used irrationally as a backfilling material in mined-out space.The work purpose was the development of a complex technology of processing the Balkhash concentrating factory's tailings (Kazakhstan) with production of a collective polymetallic concentrate and ferroalloys.The research has been fulfilled by a method of thermodynamic modelling using the software package HSC-5.1 (Outokumpy), a method of rototable experiment planning with regard to the chloride sublimation roasting of the Balkhash concentrating factory's (BCF) tailings (0.27-0.39 % of Cu; 0,54-2.03% of Zn; 0.13-0.5 % of Pb; 12.35-22.73% of Fe; 7.04-13.09% of ÑàÎ; 0.3-1.48% of MgÎ; 6.2-11.71% of Al 2 O 3 ; 0.02-0.011% of Mo; 0.04-0.07% of As; 38.49-57.99% of SiO 2 ; 0.41-0.58% of Na; 0.61-0.74% of K; 0.8-1.3% of S) and electrosmelting cinders after the roasting.It is found, that copper is extracted from the flotation tails by chloride sublimation worse, than zinc and lead.For limitation of iron chloridosublimation it is necessary to carry out the process at 7-fold oxygen excess and 3-fold CaCl 2 one.High degree of nonferrous metals' chloridosublimation (80-89 % of Cu, 95-99 % of Zn, > 99 % of Pb) and low degree of iron chloridosublimation (1-1.23 % of Fe) is observed at 1140-1200°C during 39-60 min and the surplus of CaCl 2 in 3,2 times.Electrosmelting the cinders of the chloride sublimation roasting of the Balkhash concentrating factory's (BCF) flotation tailings in a mix with coke and quartzite allows to produce a ferroalloy with silicon content of 28-63 % (at extraction in the ferroalloy of 80-87.3% of silicon).Ferrosilicon of a grade of FS50 is formed at the electrosmelting a charge containing 11 % of steel cuttings, 20 % of quartzite from the ore mass and 126-133 % of coke from a theoretically required quantity for the silicon and iron reduction.Ferrosilicon of a grade of FS45 is produced at electrosmelting the cinders in the presence of 20 % of quartzite, 6-11 % of steel cuttings and 100-106 % of coke.