Effect of Preparation Method on the Activity of Fe2O3-NiO/γ-Al2O3 Catalyst in Decomposition of Methane

2022

Full text Open access: Gold Metadata (CSL-JSON)
DOI 10.18321/ectj1435
Data confidence 70 medium
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

The effect of method preparation on the activity of Fe2O3-NiO/γ-Al2O3 catalyst was investigated in process decomposition of methane. Fe2O3-NiO/γ-Al2O3 catalyst was prepared by impregnation and solution combustion methods. The samples were characterized by X-ray phase analysis (XRD), temperature-programmed hydrogen reduction (TPR-H2), BET and Raman spectroscopy. It has been shown that the method of preparation plays an important role in regulating the textural and morphological properties of catalysts and provides a difference in their catalytic activity. The synthesis of the Fe2O3-NiO/γ-Al2O3 catalyst by the solution combustion method, in comparison with the capillary impregnation method, leads to the formation of a large amount of FeNi and FeAl2O4 solid solutions, which ensured good catalytic activity at high temperatures. The Fe2O3-NiO/γ-Al2O3 catalyst synthesized by the solution combustion method demonstrated good activity with a hydrogen yield of 52% within 150 min of the reaction without any deactivation. According to the results of Raman spectroscopy, graphene-like carbon was obtained on the surface of the catalysts. On the catalyst of Fe2O3-NiO/γ-Al2O3 (СI) synthesized by capillary impregnation, 4‒5 layer graphene on Fe2O3-NiO/γ-Al2O3 (SC)-6-7 layer graphene is formed.