Physical Processes during the Formation of Silicon-Lithium p-i-n Structures Using Double-Sided Diffusion and Drift Methods

2021

Full text Open access: Gold Metadata (CSL-JSON)
DOI 10.3390/ma14185174
Data confidence 70 medium
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

In this paper, we described a method of double-sided diffusion and drift of lithium-ions into monocrystalline silicon for the formation of the large-sized, p-i-n structured Si(Li) radiation detectors. The p-i-n structure is a p-n junction with a doped region, where the "i-region" is between the n and the p layers. A well-defined i-region is usually associated with p or n layers with high resistivities. The p-i-n structure is mostly used in diodes and in some types of semiconductor radiation detectors. The uniqueness of this method is that, in this method, the processes of diffusion and drift of lithium-ions, which are the main processes in the formation of Si(Li) p-i-n structures, are produced from both flat sides of cylindrical-shaped monocrystalline silicon, at optimal temperature (T = 420 °C) conditions of diffusion, and subsequently, with synchronous supply of temperature (from 55 to 100 °C) and reverse bias voltage (from 70 to 300 V) during drift of lithium-ions into silicon. Thus, shortening the manufacturing time of the detector and providing a more uniform distribution of lithium-ions in the crystal volume. Since, at present, the development of manufacturing of large-sized Si(Li) detectors is hindered due to difficulties in obtaining a uniformly compensated large area and time-consuming manufacturing process, the proposed method may open up new possibilities in detector manufacturing.