Porous formation process of granules from man-triggered raw materials

2019

Full text Open access: Gold Metadata (CSL-JSON)
DOI 10.1051/e3sconf/20199702025
Data confidence 70 medium
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

The results of studies of porous structure formation in a granular glass mixture are presented. Raw mixes were prepared from glass cullet, waste of magnetite ores dressing and liquid glass. The reason for adding of magnetite ores waste to the glass mixture was the information on chemical and mineral composition, results of studies of thermal transformations of waste. The rationale for adding of 20 – 30% of magnetite ores waste into the raw mix is confirmed by lowering the bloating temperature and increasing granules porosity. The effect of pyrite mineral on structural transformations in a glass mixture has been studied for the first time. It was revealed that the presence of pyrite up to 10% in the glass mixture intensifies swelling at lower temperatures. A method for preparing a molding mixture is proposed, which ensures the formation of highly porous granules with equal distribution of cells in the structure. The method involves mechanical activation of mixture of glass cullet and magnetite ores waste by grinding in a vibratory mill and subsequent portion-wise introduction of the activated mixture into liquid glass. A complex of technological methods allows obtaining porous granules with a packed density of 300 kg/m 3 at a temperature of 825°C.