Microstructure and Mechanical Properties of Equiatomic CoCrFeNiMn High-Entropy Alloy Coatings Fabricated by High-Velocity Oxygen Fuel Spraying

2026

Full text Open access: Gold Metadata (CSL-JSON)
DOI 10.3390/cryst16020103
Data confidence 70 medium
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

High-entropy coatings based on CoCrFeNiMn obtained by thermal spraying have demonstrated the potential to improve the wear resistance of traditional materials used in extreme conditions. The aim of the work was to study the effect of the oxygen/fuel ratio when using kerosene as fuel in the HVOF process on the microstructural characteristics of CoCrFeNiMn coatings, including phase composition, microhardness, elastic modulus, and wear resistance. Phase and microstructural transformations in gas-atomized powder during HVOF spraying were analyzed using XRD, SEM, and EDS methods. The tribological and mechanical properties of the coatings obtained were also evaluated. The results obtained are consistent with thermodynamic predictions based on the Scheil model for non-equilibrium conditions. The data obtained indicate the high potential of high-entropy CoCrFeNiMn alloys for use as protective coatings for industrial purposes. In addition, the results of the study emphasize the promise of using thermodynamic prediction of high-entropy alloys using Thermo-Calc software. The best mechanical and tribological properties were obtained in the HVOF 1 regime, which provided a maximum microhardness of 783.8 HV and a minimum wear rate of 7.45 × 10−5 mm3 × N−1 × m−1.