Using a rod drum mill for graphene masterbatch production

2018

Closed access Metadata (CSL-JSON)
DOI 10.1063/1.5079341
Data confidence 70 medium
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

To improve the tribological characteristics of plastic lubricants, we have previously developed a technique for modification of such substances using a graphene masterbatch. This masterbatch represents a mixture of low-viscosity oil and few-layered or multi-layered graphene obtained via graphite exfoliation. In the present work, results of masterbatch preparation in a rod drum mill due to high-gradient shear actions on a mixture of an oil base and crystalline graphite are discussed. A 2-fold decrease in the friction coeffcient was achieved when using the 1-wt% standard masterbatch or the 10-15-wt% masterbatch obtained from the graphite.