Prediction of Durability of Thermal Insulating Epoxy Coatings with Regard to Climatic Ageing

2022

Full text Open access: Gold Metadata (CSL-JSON)
DOI 10.3390/polym14091650
Data confidence 70 medium
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

It is generally accepted that the color and performance characteristics of liquid thermal insulation coatings are affected by the combined effect of various climatic factors such as solar radiation, temperature fluctuations, moisture, precipitation and others. This work presents the results of a scientific study of the full-scale exposure of coatings with regard to climatic ageing. Methods have been carried out, such as: spectrophotometry and direct scanning; determining adhesion, determining the adhesion strength of facing and protective coatings; and thermal conductivity and thermal resistance. As the results of the research work have shown, only in situ climatic tests, accompanied by the obligatory recording of the aggressive factors affecting the coating, make it possible to assess changes in the properties of epoxy coatings in full-scale conditions and, consequently, their climatic resistance by the methods of spectrophotometry and direct scanning. The ageing of polymer composites is known to be accompanied by a change not only in elasticity but also in color. Of the epoxy coatings tested, Etal-45M showed the greatest color variation during the in situ climate test. The most decorative resistant coatings are obtained using epoxy resin ED-20 + modified epoxy resin Etal-1440N.