Surface Modification of Polyethylene Terephthalate Track-Etched Membranes by 2,2,3,3,4,4,5,5,6,6,7,7-Dodecafluoroheptyl Acrylate for Application in Water Desalination by Direct Contact Membrane Distillation

Membranes, 2024

Full text Open access: Gold Metadata (CSL-JSON)
DOI 10.3390/membranes14070145
Data confidence 70 medium
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

In this work, the surfaces of poly (ethylene terephthalate) track-etched membranes (PET TeMs) with pore sizes of 670-1310 nm were hydrophobized with 2,2,3,3,4,4,5,5,6,6,7,7-dodecafluoroheptyl acrylate (DFHA) by photoinitiated graft polymerization. Attenuated total reflection FTIR spectroscopy (ATR-FTIR), scanning electron microscopy (SEM) coupled to an energy-dispersive X-ray spectrometer (EDX), and contact angle measurements were used to identify and characterize the TeMs. The optimal parameters for graft polymerization were determined as follows: polymerization time of 60 min, monomer concentration of 30%, and distance from the UV source of 7 cm. The water contact angle of the modified membranes reached 97°, which is 51° for pristine membranes. The modified membranes were tested for water desalination using direct contact membrane distillation (DCMD) method. The effects of membrane pore size, the degree of grafting, and salt concentration on the performance of membrane distillation process were investigated. According to the results obtained, it has been concluded that large pore size hydrophobic TeMs modified by using DFHA could be used for desalinating water.