Study of a Sorption Activity of the Amberlite IR120:KU-2-8 Interpolymer Systems in Relation to Dysprosium, Neodymium and Samarium Ions

2026

Full text Open access: Gold Metadata (CSL-JSON)
DOI 10.3390/polym18141780
Data confidence 85 high
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

This study investigates the sorption, structural, and morphological properties of an interpolymer system (IPS) based on Amberlite IR120 (H+) and KU-2-8 (H+) cation exchangers with acidic sulfonic groups (−SO3H), applied for the selective sorption of dysprosium (Dy3+), neodymium (Nd3+), and samarium (Sm3+) ions from aqueous solutions. The sorption activity was evaluated for seven systems with molar ratios ranging from 6:0 to 0:6 over a contact time of up to 48 h within a pH range of 2.0 to 5.0. The interpolymer pair with a molar ratio of 5:1 demonstrated the highest sorption efficiency at pH 5.0, yielding extraction degrees of 61.8% for Dy3+, 62.0% for Nd3+, and 64.4% for Sm3+. Equilibrium data were accurately described by the Langmuir isotherm model (R2 > 0.974), indicating a dominant monolayer chemisorption mechanism. The maximum monolayer adsorption capacities (qm) followed the order Dy(III) (189.59 ± 31.52 mg/g) > Sm(III) (162.27 ± 52.38 mg/g) > Nd(III) (139.90 ± 35.40 mg/g). The selectivity toward dysprosium was supported by distribution coefficients (Kd) and separation coefficients (βDy/Nd = 1.557 and βDy/Sm = 1.757 for the 6:0 system). FTIR analysis confirmed the direct coordination of lanthanide ions by sulfonic groups, as evidenced by the shifts in the νas(S=O) bands. SEM-EDX characterization revealed distinct post-sorption morphological changes (surface cracking and flaking) and confirmed significant REE accumulation on the resins (up to 4.04 wt.%) coupled with a stoichiometric decrease in sulfur content, validating the ion-exchange mechanism. These findings provide a deeper insight into the remote conformational effects governing interpolymer interactions and offer a highly promising approach for the selective recovery of REEs in hydrometallurgy.