ПРОЦЕССЫ ОБЖИГА СЫРЬЕВЫХ СМЕСЕЙ ТОО «КАСПИЙ ЦЕМЕНТ» С ДОБАВКАМИ КОМПЛЕКСНЫХ МИНЕРАЛИЗАТОРОВ

2025

Closed access Metadata (CSL-JSON)
DOI 10.54251/2616-6429.2025.02.18nu
Data confidence 70 medium
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

Высокотемпературные процессы обжига клинкера являются энергоемкими. На обжиг 1 т клинкера расходуется 110-130 кг условного топлива. Другой проблемой является загрязнение окружающей среды выбросами углекислоты. При обжиге 1 т клинкера в атмосферу выделяется до 700-800 кг СО2. Изучено влияние минерализаторов на процессы обжига сырьевых шихт ТОО «Каспийцемент». Установлено, что СаF2 и комплексные минерализаторы «СаF2 + фосфогипс» снижают температуру диссоциации, мела на 30 оС. Процессы клинкерообразования завершаются при температурах 1400 оС или на 50-100 оС ниже. Содержание СаО свободной составляет 1,2-2,0 %. Снижение температуры обжига клинкера и введение в состав сырьевой шихты фосфорных шлаков позволит уменьшить выбросы углекислоты в атмосферу, снизить загрязнение.