ИНТЕНСИФИКАЦИЯ ПРОЦЕССОВ ПОМОЛА КЛИНКЕРА ТОО «КАСПИЙЦЕМЕНТ»

2025

Closed access Metadata (CSL-JSON)
DOI 10.54251/2616-6429.2025.02.04nu
Data confidence 70 medium
How this score is calculated

It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

Исследованы процессы помола цемента при введении интенсификатора помола LS 3020. Установлено, что процесс помола цементов с добавками 0,025-0,1 % LS 3020 завершается за 25 минут тогда как без добавки цемент размалывается 35 мин. Удельная поверхность цементов с ПАВ увеличивается и составляет от 3170 см2/г до 3200 см2/г. Оптимальной является дозировка ПАВ величиной 0,025 % или 250 г на 1 т цемента. Дальнейшее увеличение дозировки добавки до 0,05 и 0,1 % не изменяет дисперсные характеристики измельчаемого цемента. Оптимальная дозировка LS 3020 не снижает прочностные характеристики цементов о чем свидетельствуют показатели прочности через 3 и 28 суток твердения, содержание химически связанной воды в гидратированном цементном камне.