It is built from checkable properties of the record itself: whether the article has a DOI, how many independent sources confirmed its data, whether the required fields are filled in, and how recent the latest confirmation is. Disagreement between sources and a missing identifier lower it. A value of 80 or above means the record was published without further checking; 60 to 79 means it is published at reduced confidence, with a manual check advisable. A record verified by an editor by hand is never pushed below 90 by a recalculation. This scores our data about the article, not the article itself.

Abstract

Cyanide-containing effluents from hydrometallurgical gold extraction pose significant environmental risks due to their high toxicity. This study investigates the detoxification of cyanide-laden tailings from the Altyntau Kokshetau gold extraction facility (Kazakhstan) using sodium percarbonate in alkaline conditions. Employing response surface methodology (RSM) and central composite design (CCD), we optimized key parameters—pH (10–12), sodium percarbonate dosage (1.5–4.0 g), reaction time (10–40 min) and temperature (20–25 °C)—achieving 83.33% detoxification efficiency within 40 min and 99.99% after 8 h, reducing cyanide from 443.2 mg/L to 0.05 mg/L. The process follows biphasic pseudo-first-order kinetics ((k1 = 0.0517) min–1 initially, (k2 = 0.01665) min–1 subsequently), driven by HO• radical-mediated oxidation of CN− to CNO−, as described by (CN−+H2O2→CNO−+ H2O). pH emerged as the dominant factor, optimizing radical stability and CN− protonation (pKa ≈ 9.21) at pH 10. Infrared spectroscopy confirmed the presence of cyanide complexes ([Au(CN)2]−, [Fe(CN)6]4−) in tailings, underscoring the need for effective treatment. The method ensures compliance with stringent environmental standards (e.g., ICMI limit of 0.2 mg/L), offering a scalable, eco-efficient solution for mitigating the environmental footprint of gold mining operations.