Аннотация
Developed consisting the explosive ammonium nitrate, paraffin and mikrosteklosfer.Due to the input of the explosive paraffin increased water resistance of explosives to 60 minutes.By entering into the explosive mikrosteklosfers been improved caking indices, since steklomikrosfers and paraffin was formed seal between the granules of ammonium nitrate.УДК 541.13 ПЕДАГОГТЫҢ КƏСІБИ ҚҰЗЫРЕТТІЛІГІН ДАМЫТУДА ЖОБАЛАУ ҚЫЗМЕТІНІҢ ОРНЫ А.Н.Каримов Əл-Фараби атындағы Қазақ ұлттық университеті, Алматы, Қазақстан e-mail: ankerimov